The short answer
To oil a deck: check it for loose boards, raised fixings and soft timber, sweep it clean, prepare the surface as the oil maker's label directs, let it dry, then apply the oil in the conditions and number of coats the label gives and keep off it until it has cured. WoodSolutions Technical Design Guide 21 (TDG 21) says a timber deck should be given a finish and kept maintained, or it will discolour, roughen, splinter and can grow mould. As a guide, penetrating oils need recoating about every 6 to 12 months, and pigmented oils last longer than clear ones. That is guidance, not a fixed rule: sun exposure and the product decide it.
Before you start
Oiling won't fix a problem in the deck, and a fresh coat can hide one. Walk the deck first and check for:
- loose, cupped or split boards;
- nails or screws standing proud of the surface;
- soft, spongy or fibrous timber, or fungal growth;
- rusted, bent or broken fixings and post brackets;
- movement in the balustrade or handrail when you push and pull on it.
The checks come from the NSW Fair Trading deck and balcony safety guide and the Queensland Government's deck inspection advice. Punching down a raised nail or replacing a screw is owner work. Rot in bearers, joists or posts, loose balustrades and stair problems are work for a licensed builder. See signs your deck needs repair.
What you need
- A broom or leaf blower.
- The deck oil, and any cleaner or preparation product the oil maker recommends.
- An applicator suited to the product: the label says which (brush, pad or roller).
- Drop sheets or tape to protect walls, paving and plants.
- Gloves and eye protection, and anything else the product's safety data sheet lists.
Step by step
- Pick your day. Check the label for the temperature range and drying conditions. Wagga averages 20.7 days a year at or above 35 °C and 21.5 frosts a year, so very hot afternoons and frosty mornings are often outside the range. Avoid days with rain forecast before the oil has dried.
- Clear and sweep. Move furniture and pots off the deck. TDG 21 recommends cleaning a deck with a broom or blower rather than a hose. Clear the gaps between boards too, so water can drain.
- Prepare the surface. If the oil maker calls for a deck cleaner or wash before recoating, use it as directed and let the boards dry fully for the time the label gives. Rough, splintered or badly weathered boards may need sanding before they will take oil evenly.
- Protect what's around the deck. Tape or cover the house wall, door frames and any paving the oil could drip onto.
- Test a small area. Try the oil on an offcut or a less visible board to check the colour.
- Apply the oil. Follow the label for how much to apply, how many coats and the time between coats. Wipe off any excess the label says should not be left on the surface.
- Let it cure. Keep foot traffic and furniture off for the time the label gives.
- Clean up safely. Follow the label's instructions for cleaning applicators and disposing of rags.
Choosing an oil
Deck oils broadly come as clear penetrating oils and pigmented (tinted) oils. WoodSolutions guidance is that penetrating oils on decks need recoating about every 6 to 12 months, and pigmented oils last longer than clear oils. When recoating, check the label says the product suits going over the finish already on the deck. If you don't know what was used before, ask the product maker or ask Addan at a quote.
Merbau has its own quirks. It is high in tannin, which can wash out as a red-brown stain on paving, and the Queensland timber database notes it can show gum bleed or oily patches that affect finishes. On a new Merbau deck, follow the supplier's advice on washing the boards before oiling. See Merbau tannin stains.
How often to oil
There is no fixed interval. As a guide:
| Situation | What to expect |
|---|---|
| Penetrating oil, full sun | Towards the 6-month end of the 6 to 12 month guide |
| Penetrating oil, shaded or covered | Towards the 12-month end |
| Pigmented oil | Longer than a clear oil |
| Finish worn through on traffic paths | Recoat, whatever the date |
The mean January maximum at Wagga is 31.9 °C, and summer UV regularly reaches the Bureau of Meteorology's extreme range. A north- or west-facing deck in full sun will wear its finish faster than one under a pergola. When the finish looks worn or the timber looks dry and faded, it is due.
Composite decks
Don't oil a composite deck unless the manufacturer's care guide says to. Composite care follows the manufacturer's instructions. See composite decking pros and cons.
Getting it done for you
Sanding and oiling are part of our deck repair work, along with replacing damaged boards. If the deck is badly weathered, Addan can check the frame, replace what needs it and bring the surface back before oiling. Call 0476 217 422 or send an enquiry for a free on-site quote.
Common questions
How often should I oil my deck?
As a guide, penetrating oils need recoating about every 6 to 12 months, and pigmented oils last longer than clear oils. A deck in full sun will need it more often than a shaded one. Recoat when the finish looks worn.
Can I oil a deck in summer?
Only within the temperature range on the product label. In Wagga that often rules out the hottest afternoons. Early mornings or cooler days are easier to work with.
Should I oil a new deck straight away?
Follow the timber supplier's and oil maker's advice. New Merbau needs its tannin dealt with first, and suppliers advise washing the boards before or soon after installation.
Do I need to sand the deck before oiling?
Not always. If the boards are rough, splintered or badly weathered, sanding helps the oil go on evenly. On a deck that has been kept up, preparation as the label directs may be all it needs.
What happens if I don't oil my deck?
TDG 21 says a timber deck without a maintained finish will discolour, roughen, splinter and can grow mould.